Amorphous Iron Formation by Discontinuous Rubbing
A layer of piled-up adherent wear debris with a thickness of more than 100 m was formed by unidirectional dry rubbing in a low vacuum, routinely removing -iron slider from -iron specimen. Large spots and halo rings can be seen